Apr 12, 2019 #1 C ChloG Community Member View Badges Joined Dec 24, 2018 Messages 74 Reaction score 37 What state or country do you live in Nebraska Rating - 0% 0 0 0 I was wondering if anyone has used krylon fusion on dry rock or concrete?
Apr 12, 2019 #2 smartwater101 Valuable Member View Badges My Tank Thread Joined Jun 14, 2018 Messages 1,762 Reaction score 2,098 Location Los Angeles What state or country do you live in California Rating - 0% 0 0 0 Yes. As long as you let it properly dry (give it a few days.) Once its dry its completely inert. If you're patient with that, it will be fine. Last edited: Apr 12, 2019
Yes. As long as you let it properly dry (give it a few days.) Once its dry its completely inert. If you're patient with that, it will be fine.
Apr 12, 2019 #3 wesman42 Valuable Member View Badges My Tank Thread Joined Apr 20, 2018 Messages 1,214 Reaction score 1,468 Location Allendale What state or country do you live in Michigan Rating - 0% 0 0 0 I personally wouldn't trust it for an underwater saltwater application. At least give the company a call.
I personally wouldn't trust it for an underwater saltwater application. At least give the company a call.
Apr 15, 2019 #4 Hermie Valuable Member View Badges My Tank Thread Joined Oct 25, 2018 Messages 2,444 Reaction score 2,621 Location Georgia OTP What state or country do you live in Georgia Rating - 0% 0 0 0 You would need to seal up the rock first with some waterproofer because the rock can erode from "behind" or under the fusion paint and the paint would flake off. What kind of rock are you talking about painting?
You would need to seal up the rock first with some waterproofer because the rock can erode from "behind" or under the fusion paint and the paint would flake off. What kind of rock are you talking about painting?